Stellite 6

S6 Material grades and equivalents: Stellite 6; UNS R30006; AMS 5387C-2001

Introduction:

Stellite 6 is the most widely used of the wear resistant cobalt-based alloys and exhibits good all-round performance. It is regarded as the industry standard for general-purpose wear resistance applications.

Stellite Chemical components

C

Cr

Si

W

Fe

Mo

Ni

Mn

B

Co

1.2

28

1.1

4.5

3

3

1

bal

*The chemical composition shown above is an outline only,and should not be taken as a full specification.
*Note that cored wire may have higher Fe contents than other product forms.

Stellite 6 Physical property (Room Temp.)

Density
(lb/in³)

Specific
Gravity

Solidus

Liquidus

Specific heat
(J/kg·K)

Magnetic
Permeability

Electrode
Potential

Electrical
Conductivity

Electrical
Resistivity

0.305

8.46

2340°F

2540°F

0.101°F
Btu/lb-

<1.2@200
Oersteds

-0.25
Volts

1.9%IACS
(Int. Annealed Copper Std.)

41.73
microhms-inch


Regular shape for all kinds of alloys

Form

Specification

Supply Form

Others

Sheet

Thickness:0.40-4.75mm,General Width:1000、1219、1500mm

Whole Coil or piece of it

Cold Annealed,Surface 2B、2E

Plate

Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled)

Whole Coil or piece of it

Single hot rolling,Solid solution annealed state,Surface 1D

Belt

Thickness:0.10-3.0mm,Width:50-500mm

Whole Coil or Specified size

Cold Annealed,Surface 2B、2E

Bar & Rod

Rolled barΦ5-45mm,Length≤1500mm

Polished Bar(circle、Square)

Solution annealing,descaling

Forged barΦ26-245mm,Length≤4000mm

Weld tube

Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm

Base on your requirement

Seamless Tube

Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm

Base on your requirement

Wire

Outer diameterΦ0.1-13mm

Base on your requirement

Ni & Ni alloy, Ti & Ti alloy

Forged piece

discs,rings,squares,blocks,slabs

Base on your requirement

Steel, Alloy

Flangs

All kinds of Flangs

Base on your requirement

Steel, Alloy

Welding Material

Coil wire Φ0.025mm-1.6mm

Base on your requirement

Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.

Straight WireΦ1.6mm-4.0mm

Welding rodΦ1.2mm-4.0mm

Tube

Elbow, three links, four links, different diameter size

Base on your requirement

Ni & Ni alloy, Ti & Ti alloy

Explosive bonded laminate

Raw Sheet Thickness≥2mm

Base on your requirement

Ni & Ni alloy, Ti & Ti alloy



Product Catalog